Hi all.
Glad to be part of the club
I currently have a dilema regarding the removal of 88tungsten-carbide-8Cobalt-4Chromium coatings which are between 4 and 5 thou thick.
I found some previous articles on this site which suggested Enstrip-317GT but unfortunately, after many trials, the results were not encouraging. I think the problem relates to the Cobalt-Chromium constituents in the coating because 317GT should be very effective at stripping WC.
I know that electrolytic processes are probably the best option but as this is a new trial, the cost of buying the neccessary equipment is too great.
Our testing abilities include the option to introduce temperature and aggitation to products immersed within solution.
Any help and advice is very well appreciated
All the best, Batsy.