Tungsten Carbide coating
05-25-2010, 10:33 AM,
#1
Tungsten Carbide coating
Hi everyone,
I understand that that WC based coatings is to be used in the environment where the temperature is to be below 500'C. Is it because of decarburization or oxidation which make the coating fails?
2nd, In HVOF process e.g Dj2600 how the decarburization is minimized/eliminated where the powders are fed into combustion chamber which is around 2000'C or more?. Do the combustion melt Cobalt only and what transformation takes place for WC?
By the way practically I get good coating, just want to know what happens and explained theoritically.

Thank you
Reply
05-25-2010, 07:54 PM,
#2
RE: Tungsten Carbide coating
Hi Guna

Quote:I understand that that WC based coatings is to be used in the environment where the temperature is to be below 500'C. Is it because of decarburization or oxidation which make the coating fails?

Yes

Quote:2nd, In HVOF process e.g Dj2600 how the decarburization is minimized/eliminated where the powders are fed into combustion chamber which is around 2000'C or more?. Do the combustion melt Cobalt only and what transformation takes place for WC?

Ideally, the particles are heated just enough to allow splatting on impact (not necessarily melting) and not high enough to cause reaction/alloying between WC and cobalt or oxidation/decarburisation. Fortunately, HVOF's very high velocity limits the particles dwell/heating time dramatically and allows use some control when using suitably sized particles.

details-on-hvof-t-1013.html
Reply




Possibly Related Threads…
Thread Author Replies Views Last Post
  Tungsten Carbide Microfinish engineerraj 15 16,874 02-17-2023, 09:41 PM
Last Post: J!m
Photo Pitting in HVOF Tungsten Carbide mrobie 4 2,425 08-31-2022, 02:08 PM
Last Post: Red Baron
  Request for solution to reduce porosity in HVOF Tungsten Carbide Coatings sreenuvundela 7 12,380 07-22-2020, 08:01 AM
Last Post: Simon Kim
  Tungsten Carbide HVOF Removal PrecisionCarbide 9 14,295 02-24-2020, 11:17 AM
Last Post: Packiaraj Mutharasu
  Chrome-Carbide coating issue DanyGans 11 10,544 10-08-2019, 05:19 PM
Last Post: Lemster68
  remove tungsten coating gito 1 2,403 03-22-2019, 10:12 PM
Last Post: sprayloud
  roller surface high roughness Tungsten carbide coating Ra 0.15-0.3mm zhuminkun 6 5,170 02-08-2019, 04:59 AM
Last Post: Taz
  strange ring shaped grooves in carbide coating DavidH 3 3,493 08-21-2017, 02:01 PM
Last Post: DavidH
  Dark surface after grinding of plasma tungsten carbide coating Lazha 1 3,779 05-31-2017, 12:07 PM
Last Post: loriolo
  HVAF tungsten carbide to replace hard chrome - Help??!!! Adamreis 2 4,187 02-20-2017, 11:04 PM
Last Post: Vig
  Effective Way of Testing hardness of Tungsten Carbide MANGESH 2 7,450 12-03-2015, 09:25 PM
Last Post: alaskangrown
  Tungsten Carbide coatings Sealants sorousheti 5 7,910 11-23-2015, 10:18 AM
Last Post: sorousheti
  Boron Carbide as a Surface Coating TCHP222 0 3,803 11-12-2015, 08:06 PM
Last Post: TCHP222
  Cold Spray with Tungsten Carbide LLBHW 3 12,780 04-24-2015, 01:06 AM
Last Post: Fermit
  HVOF Tungsten Carbide - New Line Setup David 1 5,040 08-16-2014, 03:51 PM
Last Post: Gordon



Users browsing this thread: 1 Guest(s)





Surface Engineering Forum Sponsor - Alphatek Hyperformance Coatings Ltd