roller surface high roughness Tungsten carbide coating Ra 0.15-0.3mm
05-15-2018, 01:16 PM,
#1
roller surface high roughness Tungsten carbide coating Ra 0.15-0.3mm
hello, every expertise, need your input or idea, how i can make roller surface roughness Ra 0.15-0.3mm

per my understanding, when we machine the roller we need to kepp 0.2mm Ra then this may happen. any ideas or procedure you can suggest will be 120% appreciate.
Reply
05-15-2018, 02:49 PM,
#2
RE: roller surface high roughness Tungsten carbide coating Ra 0.15-0.3mm
(05-15-2018, 01:16 PM)zhuminkun Wrote: hello, every expertise, need your input or idea, how i can make roller surface roughness Ra 0.15-0.3mm

per my understanding, when we machine the roller we need to kepp 0.2mm Ra then this may happen. any ideas or procedure you can suggest will be 120% appreciate.

You need flame spraying or plasma spraying of a powder mixture of self-fluxing nickel-based alloy + tungsten-molten carbide (NiCrBSi + WC/W2C). If the grain size of your carbide is 0.2-0.5 mm, you will get a coating roughness of 0.1-0.3 mm.
Reply
05-16-2018, 01:47 PM,
#3
RE: roller surface high roughness Tungsten carbide coating Ra 0.15-0.3mm
(05-15-2018, 02:49 PM)Vadim Verlotski Wrote:
(05-15-2018, 01:16 PM)zhuminkun Wrote: hello, every expertise, need your input or idea, how i can make roller surface roughness Ra 0.15-0.3mm

per my understanding, when we machine the roller we need to kepp 0.2mm Ra then this may happen. any ideas or procedure you can suggest will be 120% appreciate.

You need flame spraying or plasma spraying of a powder mixture of self-fluxing nickel-based alloy + tungsten-molten carbide (NiCrBSi + WC/W2C). If the grain size of your carbide is 0.2-0.5 mm, you will get a coating roughness of 0.1-0.3 mm.

Tks Vadim, i will ask vendor to make some test samples.
Reply
05-20-2018, 06:15 AM,
#4
RE: roller surface high roughness Tungsten carbide coating Ra 0.15-0.3mm
Pre grinding-Pre honing - Chrome Plating- Final Grinding and Final Honing

or As Vadim mentioned below... flame spraying or plasma spraying of a powder mixture of self-fluxing nickel-based alloy + tungsten-molten carbide (NiCrBSi + WC/W2C)
Pre grinding -Flame / Plasma Spray- Final Grinding (Diamond wheel) and Super Polishing

How ever, If it is chrome plating you required Honing / fro Thermal Spray you need to do super polishing to achieve 0.1 Ra
Reply
01-31-2019, 12:25 PM,
#5
RE: roller surface high roughness Tungsten carbide coating Ra 0.15-0.3mm
Hello, which mesh do you recommend to spray with hvof to achieve 250 micro inch Ra after spraying?
88WC 12CO powder
How do we prepare the surface?
We have to spray bridle rolls
Reply
02-01-2019, 10:35 PM, (This post was last modified: 02-01-2019, 10:37 PM by Met.Eng..)
#6
RE: roller surface high roughness Tungsten carbide coating Ra 0.15-0.3mm
Hi zhuminkun,

You may spray with ArcSpray system under WC coating for high Ra Wink
Reply
02-08-2019, 04:59 AM,
#7
RE: roller surface high roughness Tungsten carbide coating Ra 0.15-0.3mm
Is there any HVOF coating that we can get below Ra 2.0 mm?
Reply




Possibly Related Threads…
Thread Author Replies Views Last Post
  Request for solution to reduce porosity in HVOF Tungsten Carbide Coatings sreenuvundela 7 8,788 07-22-2020, 08:01 AM
Last Post: Simon Kim
  Tungsten Carbide HVOF Removal PrecisionCarbide 9 9,168 02-24-2020, 11:17 AM
Last Post: Packiaraj Mutharasu
  Chrome-Carbide coating issue DanyGans 11 6,434 10-08-2019, 05:19 PM
Last Post: Lemster68
  surface speed for HVOF coating process gito 8 2,109 05-03-2019, 01:08 PM
Last Post: Lemster68
  remove tungsten coating gito 1 1,073 03-22-2019, 10:12 PM
Last Post: sprayloud
  Coating for cyclone internal surface Arturas 0 798 12-11-2018, 06:58 AM
Last Post: Arturas
  Roller bearing KevGarty 2 1,520 02-07-2018, 09:43 PM
Last Post: demionkrishan
  Coating surface roughness William 9 21,040 12-26-2017, 10:40 AM
Last Post: Vadim Verlotski
  Powder Coating for Surface Table achmadarifudinh 3 2,076 11-28-2017, 12:19 PM
Last Post: Artyom
  strange ring shaped grooves in carbide coating DavidH 3 1,904 08-21-2017, 02:01 PM
Last Post: DavidH
  Dark surface after grinding of plasma tungsten carbide coating Lazha 1 2,148 05-31-2017, 12:07 PM
Last Post: loriolo
  HVAF tungsten carbide to replace hard chrome - Help??!!! Adamreis 2 2,462 02-20-2017, 11:04 PM
Last Post: Vig
  Un-common surface pattern on coating failure shantanu 2 2,216 10-06-2016, 02:55 PM
Last Post: Vig
  Effective Way of Testing hardness of Tungsten Carbide MANGESH 2 4,786 12-03-2015, 09:25 PM
Last Post: alaskangrown
  Tungsten Carbide coatings Sealants sorousheti 5 5,117 11-23-2015, 10:18 AM
Last Post: sorousheti



Users browsing this thread: 1 Guest(s)





Surface Engineering Forum Sponsor - Alphatek Hyperformance Coatings Ltd