Posted by Gordon England on May 09, 2003 at 16:57:52:
In Reply to: Re: Rockwell Vs. UTS posted by Michael Doyle on May 09, 2003 at 16:44:20:
: Hi Gordon,
: The 304 SS wire has been cold work hardened by drawing it through a die.
Hi Michael
Have you got the 420 in the same wire size? Simple qualitative test - try snipping wires with some wire cutters, you should readily feel which is harder by the effort required.
Follow Ups: