I have a question about the material of sink roll.
SS316L FERRITE FREE. Ferrite free means the SS316L will be austenite after annealed (how long?), then no magnetic. Am I right?
www.cnmaker.com, sink roll for galvanizing line or Al-Zn-Si line.[/u]
Reply
01-05-2010, 07:24 PM,
#2
RE: about Ferrite free for sink roll
Hi nettrade

Sign0016 to the Surface Engineering Forum.

Ferrite phase tends to be ferromagnetic, austenite phase tends to be non-magnetic. so yes you are right Smile
Reply
01-06-2010, 02:02 AM,
#3
RE: about Ferrite free for sink roll
(01-05-2010, 07:24 PM)Gordon Wrote: Hi nettrade

Sign0016 to the Surface Engineering Forum.

Ferrite phase tends to be ferromagnetic, austenite phase tends to be non-magnetic. so yes you are right Smile

Hi Gordon,

Thank you for your reply.
www.cnmaker.com, sink roll for galvanizing line or Al-Zn-Si line.[/u]
Reply




Possibly Related Threads…
Thread Author Replies Views Last Post
  Looking for free standard codes? manganow 0 2,939 01-04-2012, 02:08 AM
Last Post: manganow
Bell Sink roll for Galvanizing line or Al-Zn-Si line nettrade 2 6,182 01-13-2010, 03:31 AM
Last Post: nettrade



Users browsing this thread: 1 Guest(s)





Surface Engineering Forum Sponsor - Alphatek Hyperformance Coatings Ltd