The conditions of deposition of CoNiCrAl+Si at the HVOF
09-20-2018, 07:37 AM,
#1
The conditions of deposition of CoNiCrAl+Si at the HVOF
Hello everyone!
I want to apologize for my English. I hope you will understand me: Ashamed0002:
Dear colleagues, will you be so kind to help me!

I work with WokaJet-410-S.
What requirements must be met for spraying CoNiCrAl+Si at the HVOF?
Interested to what temperature must you heat the blade?
What temperature should be when spraying?
What should be the lambda? 1.05?
Thanks for your help!
Reply




Possibly Related Threads…
Thread Author Replies Views Last Post
  Electron-beam physical vapor deposition masking jtonic77 6 3,804 10-04-2022, 06:31 PM
Last Post: SakshiVerma
  Electro Spark Surface Deposition Machine Met.Eng. 2 7,278 09-12-2014, 05:43 PM
Last Post: plasmajet1990
  Effect of weather on deposition efficiency Max K 3 5,905 08-06-2013, 04:40 PM
Last Post: GMA thermal spray systems
  Molybdenum deposition on copper plasmajet1990 9 9,548 06-04-2013, 09:07 PM
Last Post: plasmajet1990
  Better deposition without changing parameters and feedrate? Pnewbie 5 8,435 02-03-2012, 01:16 AM
Last Post: LEN WOOD
  Measuring deposition efficiency and check the microstructures of the coatings??????? fahad03092 7 11,012 10-25-2011, 02:05 PM
Last Post: djewell
  Deposition effect of Metco 42C Met.Eng. 5 10,035 08-11-2011, 03:10 AM
Last Post: Gordon
Question obstruction during deposition of amorphous powders desMoira 6 7,799 07-22-2010, 01:18 PM
Last Post: desMoira
  Deposition efficiency of Metco 131VF raviswanadha 3 8,369 03-28-2009, 02:52 PM
Last Post: Gordon
Lightbulb Resin for tough conditions LeeWL 4 5,769 02-26-2009, 01:25 AM
Last Post: Gordon
  Deposition Efficiency Measurement deepskysea 3 9,291 09-05-2008, 02:38 PM
Last Post: Gordon



Users browsing this thread: 1 Guest(s)





Surface Engineering Forum Sponsor - Alphatek Hyperformance Coatings Ltd