Hi Frank
to the Surface Engineering Forum.
Quote:How to improve adhesion before starting the fusing step?
Preheating, which temperature?
May help if we knew more about your equipment /set-up and what specific problems you want to address.
Quote:Selffluxing Bond layer?
If you are talking about using a similar but softer/more ductile self-fluxing alloy as a base coat, then this can be good system for thicker coatings or where you need to reduce the thickness of a more troublesome top layer.
Quote:mass flow oxygen and acetylene?
Equipment/powder?