Masking tape or compounds suggestion
03-02-2015, 10:11 AM,
#1
Masking tape or compounds suggestion
Hi everyone,
is anyone have suggestion for masking compounds or some masking materials for small holes diameter 0.64-0.76mm. I need to applicate Metco 204B-NS coating on surface where are small holes and i need to save holes from powder becouse i do not have facility to drill holes again. Here is the pictures of example.

Best regards, Sasa Golubovic.
   
   
Reply
03-10-2015, 07:01 AM,
#2
RE: Masking tape or compounds suggestion
(03-02-2015, 10:11 AM)texnicar Wrote: Hi everyone,
is anyone have suggestion for masking compounds or some masking materials for small holes diameter 0.64-0.76mm. I need to applicate Metco 204B-NS coating on surface where are small holes and i need to save holes from powder becouse i do not have facility to drill holes again. Here is the pictures of example.

Best regards, Sasa Golubovic.

I've ever used a soft matireial like plasticine years ago which is from Sulzer in Switzerland. But I don't remember the name. It is pink and soft and it can resist the impact of plasma flame.
Maybe you can try to contact with them to see if they have any infomation.
Reply
03-14-2015, 12:00 AM, (This post was last modified: 03-14-2015, 12:02 AM by loriolo.)
#3
RE: Masking tape or compounds suggestion
Hi......
Use graphite sticks like for pencil, you can buy them at a stationery store, there are 0,5mm/0,75mm and 1mm or more., in some case i used copper wire, this because on copper the coating do not bond easily, take care apply without sand blasting the copper, plece the copper wire after sand blast operation.
Best regards
Luigi
Reply
03-16-2015, 03:15 AM,
#4
RE: Masking tape or compounds suggestion
This is what I used at Turbocare and Siemens.

https://www.dymax.com/adhesives/products/718

It works amazing for cooling holes of any size.
Reply
03-18-2015, 12:36 PM,
#5
RE: Masking tape or compounds suggestion
In the high Temperature Brazing Industry they use a slurry to fill the whole Cavity on Turbine parts with Cooling holes to prevent melting Brazing Filler Metal from entering the Holes during Brazing process.
I can supply a small sample for testing.
If interested I will explain Procedure in more detail.
Reply




Possibly Related Threads…
Thread Author Replies Views Last Post
  HVAF Masking TimHewitt1 3 2,250 12-11-2019, 06:45 PM
Last Post: JJStick
  Need help with masking materials search Artyom 2 957 04-20-2019, 07:18 AM
Last Post: loriolo
  Plasma Spray Masking Tape achmadarifudinh 2 1,251 09-06-2018, 02:48 AM
Last Post: achmadarifudinh
  Gas Turbine Blades HVOF Coating masking demionkrishan 7 4,487 01-17-2018, 01:09 AM
Last Post: Taz
  HVOF masking demionkrishan 2 3,021 01-15-2016, 02:29 PM
Last Post: demionkrishan
  Masking tape for high-heat ceramic coating. texnicar 1 2,688 04-21-2015, 04:09 PM
Last Post: cris1904
  HVOF masking Kopi81 9 8,438 04-09-2015, 09:01 PM
Last Post: giuiori75
  plasma hard masking vendors CHI3 2 4,112 03-16-2015, 03:20 AM
Last Post: Meeker77
  Masking of Cooling Holes gshejale 4 6,327 01-20-2008, 10:09 PM
Last Post: plasmajet1990



Users browsing this thread: 1 Guest(s)





Surface Engineering Forum Sponsor - Alphatek Hyperformance Coatings Ltd