Good preparation for cast iron base material
11-23-2016, 01:01 AM,
#1
Good preparation for cast iron base material
Dear Friends,

Does anybody has good experiences for surface preparation for Cast Iron base materials, now our sand blasting (24#WA,4.5 bar air)process is not enough to increase surface situation, roughness of the substrate is not good, and seems contamination on the interface when check the metallographic after coating, so it is not for the bond strength, thanks!Shy

B.R

Reply
11-23-2016, 09:55 AM,
#2
RE: Good preparation for cast iron base material
(11-23-2016, 01:01 AM)plzc126330 Wrote: Dear Friends,

Does anybody has good experiences for surface preparation for Cast Iron base materials, now our sand blasting (24#WA,4.5 bar air)process is not enough to increase surface situation, roughness of the substrate is not good, and seems contamination on the interface when check the metallographic after coating, so it is not for the bond strength, thanks!Shy

B.R

As far as i know you might have to "bake" it at elevated temperatures to burn out oil residue prior to grit blasting.
Reply
11-23-2016, 06:25 PM,
#3
RE: Good preparation for cast iron base material
(11-23-2016, 01:01 AM)plzc126330 Wrote: Dear Friends,

Does anybody has good experiences for surface preparation for Cast Iron base materials, now our sand blasting (24#WA,4.5 bar air)process is not enough to increase surface situation, roughness of the substrate is not good, and seems contamination on the interface when check the metallographic after coating, so it is not for the bond strength, thanks!Shy

B.R

Hi
what kind of cast iron is it?
hardness of base?
Is it new or used somewhere ( then where) cast iron?
spray gun?
coating type, properties of the coating you need to spray?


Reply
11-24-2016, 01:17 AM, (This post was last modified: 11-24-2016, 01:24 AM by plzc126330.)
#4
RE: Good preparation for cast iron base material
(11-23-2016, 09:55 AM)Corund Wrote:
(11-23-2016, 01:01 AM)plzc126330 Wrote: Dear Friends,

Does anybody has good experiences for surface preparation for Cast Iron base materials, now our sand blasting (24#WA,4.5 bar air)process is not enough to increase surface situation, roughness of the substrate is not good, and seems contamination on the interface when check the metallographic after coating, so it is not for the bond strength, thanks!Shy

B.R

As far as i know you might have to "bake" it at elevated temperatures to burn out oil residue prior to grit blasting.

Dear Colud,

Thanks a lot for your comments, I also try to preheat the products (piston ring) with flame torch, so as your experiences, how about the temp could good or enough to sand blasting, I using 20# WA, thanks again.

B.R
(11-23-2016, 06:25 PM)Arturas Wrote:
(11-23-2016, 01:01 AM)plzc126330 Wrote: Dear Friends,

Does anybody has good experiences for surface preparation for Cast Iron base materials, now our sand blasting (24#WA,4.5 bar air)process is not enough to increase surface situation, roughness of the substrate is not good, and seems contamination on the interface when check the metallographic after coating, so it is not for the bond strength, thanks!Shy

B.R

Hi
what kind of cast iron is it?
hardness of base?
Is it new or used somewhere ( then where) cast iron?
spray gun?
coating type, properties of the coating you need to spray?

Reply




Possibly Related Threads…
Thread Author Replies Views Last Post
Video Repair of base material defect after HVOF Coating Pranab_hvof 2 4,637 06-27-2022, 12:20 PM
Last Post: sushil1405
Star HVOF WCCo on Chilled Cast Iron(55HRC) tobjung 1 2,142 03-04-2021, 11:16 AM
Last Post: Vadim Verlotski
  Ceramic Coating on Aluminum Base metal demionkrishan 9 4,841 02-03-2020, 09:35 AM
Last Post: DMan
  WC-CO-CR hvof coating thickness measurement on Base SS 316L JRB VIRANI 3 3,155 06-20-2019, 09:16 AM
Last Post: loriolo
  Substrate preparation VS bonding strength plzc126330 2 3,400 01-09-2018, 03:48 AM
Last Post: plzc126330
  Bonding coating for Cast steel subsrate plzc126330 5 5,688 08-15-2016, 09:01 AM
Last Post: plzc126330
  Cast iron restoring sprayloud 1 3,230 04-11-2016, 12:54 AM
Last Post: aerotherm
  Surface Preparation of Aluminium acidic 2 4,894 05-09-2015, 01:59 PM
Last Post: CHI3
Question Brown aluminum oxide VS Chilled iron grit Bacon 2 4,830 03-27-2015, 06:23 PM
Last Post: Bacon
  Cast iron powder or wire M.Naguib 4 6,162 12-08-2013, 12:14 AM
Last Post: kschewe
  Spray and Fuse Co-base or Ni-base alloy on Inconel 718 Frank 1 4,264 09-23-2012, 01:12 PM
Last Post: Gordon
  metallographic preparation volf 2 7,656 01-25-2012, 12:48 PM
Last Post: jonini
  Surface preparation before spraying HVOF minh_8888 4 9,532 06-20-2011, 12:18 PM
Last Post: Met.Eng.
  Solvent Resistant Sealers - Know of any good ones? MichiganMan 2 4,145 04-07-2011, 02:10 PM
Last Post: MichiganMan
  Surface Preparation Coolguy 3 5,417 02-08-2011, 07:47 PM
Last Post: MichiganMan



Users browsing this thread: 1 Guest(s)





Surface Engineering Forum Sponsor - Alphatek Hyperformance Coatings Ltd