Deposit Efficiency
Hello All,

Trying to get better deposit efficiency using Sg-100 with argon primary and nitrogen secondary. Parameters of 110 psi on Argon and 60 psi on Nitrogen,and 40 psi on carrier gas. Running at 650 amps around 46 volts.
The coating looks good and clean but DE is off around 15%. Standoff is at
4". Wondering if I've got to much velocity. Any suggestions would be appreciated. Joe
Reply
08-28-2012, 07:34 PM,
#2
RE: Deposit Efficiency
Hi Joe

I think we will need more info to comment. What powder are you spraying? and are you using a recommended parameter set for equipment and powder?

Quote:The coating looks good and clean but DE is off around 15%.

I'm unclear as to whether you mean you are getting 15% deposit efficiency which is very low or that you mean 15% deviation from an expected level.
Reply
09-03-2012, 04:05 PM,
#3
RE: Deposit Efficiency
If D.E. is around 15%, you are having a very poor efficiency, becouse ussually you can get from 60 to 90 %, depend of the powder and thermalspray equipment been used.
Best regards
Luigi
Reply




Possibly Related Threads…
Thread Author Replies Views Last Post
  How do you caculate deposit efficiency of thermal spray derek 2 6,832 02-25-2014, 08:10 PM
Last Post: Gordon
  Effect of weather on deposition efficiency Max K 3 5,881 08-06-2013, 04:40 PM
Last Post: GMA thermal spray systems
  HELP TO DEPOSIT SPRAY & FUSE COATING OF STELLITE POWDER --- REG sreenuvundela 10 14,252 03-14-2012, 11:46 AM
Last Post: Vijay Deshpande
  Measuring deposition efficiency and check the microstructures of the coatings??????? fahad03092 7 10,989 10-25-2011, 02:05 PM
Last Post: djewell
Shy What is the main factor for affecting the efficiency of melting the powder? Justin 8 8,974 09-26-2011, 06:03 PM
Last Post: sreenuvundela
Question Can rate of deposit be calculated? junebrooks 1 4,399 09-07-2009, 03:20 PM
Last Post: Gordon
  Deposition efficiency of Metco 131VF raviswanadha 3 8,342 03-28-2009, 02:52 PM
Last Post: Gordon
  Deposition Efficiency Measurement deepskysea 3 9,280 09-05-2008, 02:38 PM
Last Post: Gordon
  how to increase TBC deposit speed? derek 11 17,405 05-06-2008, 11:26 PM
Last Post: hvofhamid
  increase efficiency of LTH (Laser Transformation Hardening) melrose 1 6,978 06-18-2007, 04:30 PM
Last Post: Gordon



Users browsing this thread: 1 Guest(s)





Surface Engineering Forum Sponsor - Alphatek Hyperformance Coatings Ltd