Post Reply 
metalllizing tugboat
09-23-2006, 07:42 PM
Post: #1
metalllizing tugboat
hello everybody

two questions
first . can you give me how many kilos of zn/al per square meter for a tickness of 250 ??
second. how many hours work a nozzle before to change (average)?
regards
thierry
Find all posts by this user
Quote this message in a reply
09-24-2006, 12:36 AM
Post: #2
RE: metalllizing tugboat
Hi thierry

1.725 kg per square metre at 250 micrometres thick. Based on Metco technical bulletin for Metco Zinc-Al 85/15 alloy wire and 10E gun (wire req'd per unit of coating 0.0069 kg/cubic centimetre).

Sorry, I don't know answer to second question.

Regards Gordon
Visit this user's website Find all posts by this user
Quote this message in a reply
09-24-2006, 08:12 AM (This post was last modified: 02-12-2007 03:09 PM by Gordon.)
Post: #3
RE: metalllizing tugboat
thanks for info,bye
thierry
Quote:Hi thierry

1.725 kg per square metre at 250 micrometres thick. Based on Metco technical bulletin for Metco Zinc-Al 85/15 alloy wire and 10E gun (wire req'd per unit of coating 0.0069 kg/cubic centimetre).

Sorry, I don't know answer to second question.
Find all posts by this user
Quote this message in a reply
10-05-2007, 03:26 PM
Post: #4
RE: metalllizing tugboat
Hi Theirry,

Are you looking to purchase any zinc/aluminum for metallizing?

Thanks

Danns
Find all posts by this user
Quote this message in a reply