Gordon,

I have a question on the tolerance capability level for thermal spray processes
.I would like to know, what is the best tolerance (i.e. +/- 0.00x) that can be achieved with HVOF or Air Plasma?

For my process
1. APS - I could achieve a deposition rate in the range of 0.001"~0.003" per pass.
2. HVOF - I could achieve a deposition rate in the range of 0.00025 ~0.0005
Any information would be appreciated!

Thanks.

Regards,
Alex
Reply
12-17-2016, 10:55 PM,
#2
RE: Thermal Spray Tolerance Limit
Hi Alex

It seems that you need some little training, every material has his own deposition rate, as well as it is an important issue to consider during the parameters selection for every powder, of course ther isn't a global or best general deposition range.
Best regards
Luigi
Reply




Possibly Related Threads…
Thread Author Replies Views Last Post
  Powder stabilization time and coating time limit nicholasktc 1 1,808 06-25-2020, 12:59 PM
Last Post: Lemster68
  Surface contact stress limit over an HVOF coating HVoilF 1 5,174 05-22-2013, 02:07 PM
Last Post: djewell
  center line tolerance. RVRTRSH 5 7,646 11-02-2009, 04:24 PM
Last Post: RVRTRSH
  Thermal Spray Tolerance Limit Alexangel1226 8 14,606 12-24-2007, 06:46 PM
Last Post: hvofhamid



Users browsing this thread: 1 Guest(s)





Surface Engineering Forum Sponsor - Alphatek Hyperformance Coatings Ltd