Fusing and heat treatment
06-22-2017, 04:59 AM,
#1
Fusing and heat treatment
Lets say i would spray fuse NiCrBSi coating on tool steel substrate.
After i would heat treat steel to 60HRC.
How would this heat treatment affect coating properties ?
Reply
06-22-2017, 06:46 AM,
#2
RE: Fusing and heat treatment
(06-22-2017, 04:59 AM)sprayloud Wrote: Lets say i would spray fuse NiCrBSi coating on tool steel substrate.
After i would heat treat steel to 60HRC.
How would this heat treatment affect coating properties ?
It works quite well if you have the temperature of the heat treatment below 1000°C. In this case, there is no damage to the layer.
Reply
06-23-2017, 07:26 AM,
#3
RE: Fusing and heat treatment
I am asking because i got a drop in hardness of the coating by ~8HRC.
Could this happen if the temperature was >1000C ?
Reply
06-24-2017, 12:30 PM,
#4
RE: Fusing and heat treatment
(06-23-2017, 07:26 AM)sprayloud Wrote: I am asking because i got a drop in hardness of the coating by ~8HRC.
Could this happen if the temperature was >1000C ?

When the temperature of the heat treatment exceeds 1040°C, the layer is partially melted. This melt is an eutectic in the Ni-Cr-B-Si system and contains much boron and silicon which are responsible for the hardness of the layer. Thus, when this eutectic melt flows away from the part, more nickel and fewer boron and silicon remain in the layer as compared with the pre-heat treatment state. Loss of boron and silicon also means loss in the hardness of the layer.
Reply




Possibly Related Threads…
Thread Author Replies Views Last Post
  Fusing process candierosa 1 1,983 04-08-2023, 06:40 AM
Last Post: Vadim Verlotski
  Fusing Process: Frame Spray vs Plasma Spray tobjung 2 1,171 09-07-2022, 01:22 PM
Last Post: Gordon
  Surface Treatment of Ceramic Coatings brkozdemir41 0 1,937 12-18-2020, 12:09 AM
Last Post: brkozdemir41
  heat treatment of MCrAlY coatings clover 4 8,102 06-26-2017, 12:55 PM
Last Post: Nesher
  Coating and Heat treatment Improvements demionkrishan 2 2,853 04-22-2017, 06:13 AM
Last Post: demionkrishan
  Heat treatment after HVOF process to decrease porosity Giroud 3 6,239 07-13-2015, 05:51 AM
Last Post: aerotherm
  Masking tape for high-heat ceramic coating. texnicar 1 4,136 04-21-2015, 04:09 PM
Last Post: cris1904
  Metco 16C-NS fusing problem Sprayman12 4 9,778 10-08-2014, 08:04 PM
Last Post: Met.Eng.
  Sprayed, welded or cast alloys for high heat Zanitech 2 4,050 10-01-2013, 09:08 PM
Last Post: Met.Eng.
  Chrome Carbide & T800 Coating Property Change after heat treatment Alexangel1226 5 14,704 09-30-2010, 03:04 AM
Last Post: arjfaye06
  surface treatment of Pistols sadaqat 3 5,611 01-09-2010, 05:37 PM
Last Post: Gordon
  Renew plasma after heat treatement TurbineRepair 3 6,886 10-14-2008, 09:52 AM
Last Post: Alexangel1226
  Heat Treatment of Abradable Coatings wasif 1 5,113 09-04-2007, 03:59 PM
Last Post: Gordon
  Preheating heat sources powerman 2 6,185 07-29-2007, 12:19 AM
Last Post: powerman
  Fusing of cast iron Arturas 1 6,966 08-16-2006, 01:23 PM
Last Post: Gordon



Users browsing this thread: 1 Guest(s)





Surface Engineering Forum Sponsor - Alphatek Hyperformance Coatings Ltd