Posted by Paul Burkhardt (207.206.58.254) on 14:35:56 15/11/04

In Reply to:Re: Flaws in stellite coatings posted by Gordon England

The coating is Stellite #6, it is plasma arced onto stainless steel type 316.
Would the fact that the machining involves an intermittent cut cause a problem? (This is machining an off-set cone profile onto the seat).