In Reply to:Use of coating above 1700K posted by Hanamantray Baluragi

: Kindly suggest me a proper coating that can withstand 1700K and thickness of coating required

: regards
: Hanamantray

Coatings with melting point in excess of 1700K. Choice and thickness will depend on environment and purpose of coating.

Regards Gordon