: Daniel. Thanks 86WC/Co10/Cr4,not Co4/Cr10. hope someone can let me know their thoughts on dissolving cobalt when it is in the sprayed state.

Hi Daniel

What is your purpose in dissolving the cobalt?

Dissolving all cobalt selectively may be very difficult as the cobalt may be present in many different combinations with the other constituents.

Regards Gordon